Solution process for the production of ep(d)m elastomers and polymerisation reactor for use in said process.

作者: Gabriele Omicini

DOI:

关键词:

摘要: The invention describes a process for the production of EP(D)M in solution stirred reactor (CSTR) which reaction bath is kept boiling condition at temperature between 40 and 60° C. pressure 0.6 1.3 MPa, from 40% to 80% heat removed by remaining subcooling fluids recycled reactor. provided with stirring system three impellers, device distribution bottom gamma ray level control device.

参考文章(11)
Alec Y. Wang, Pradeep Jain, Nile A. Mead, Job D. Guzman, Robert D. Swindoll, Prasanna K. Jog, Polymerization process for olefin-based polymers ,(2010)
Jon Edmond Stanat, Linda Kay Wright, Robert Martin Koros, Harold Wilbur Margo, Kenneth Lee Kaufman, Albert Rossi, Salvatore Rea, Jeffery William Frederick, Dilute process for the polymerization of ethylene/alpha-olefin copolymer using metallocene catalyst systems ,(1993)
Periagaram Srinivasan Ravishankar, Elastomeric reactor blend compositions ,(2005)
Hidetake Hozumi, Hisakatsu Hama, Process for producing ethylene -alpha- olefin copolymer ,(2008)
Rinaldo Soria Schiffino, Javier Mario Zamora, Ethylene-.alpha.-olefin/diolefin polymer solution polymerization process ,(1996)