作者: Sui Lin Shi , Wei Pan , Ming Hao Fang , Zhen Yi Fang
DOI: 10.1111/J.1551-2916.2005.00764.X
关键词:
摘要: Ti3SiC2/HAp composites with different Ti3SiC2 volume fractions were fabricated by spark plasma sintering (SPS) at 1200°C. The effects of addition on the mechanical properties and microstructures investigated. bending strength fracture toughness increased increasing content, whereas Vickers hardness decreased. reached 252±10 MPa 3.9±0.1 MPa·m1/2, respectively, 50 vol% Ti3SiC2. increases in attributed to matrix strengthening interactions between cracks platelets.