作者: M. B. Thomas , R. H. Doremus , M. Jarcho , R. L. Salsbury
DOI: 10.1007/BF00552099
关键词:
摘要: Dense hydroxylapatite was examined with the diametral test at different loading rates, after treatment in solutions, and under static load. The fatigue tests showed that is quite resistant to as compared other oxides. simple Weibull distribution of strengths not obeyed. Different solution treatments implanting did appreciably change its strength.