Grinding of cemented carbide with electrical spark assistance

作者: Philip Koshy , V.K Jain , G.K Lal

DOI: 10.1016/S0924-0136(97)00130-1

关键词:

摘要: … With these mechanisms operative, the wear volume was found to have a good correlation with the product of hardness and fracture toughness of the specimen. Under repeated …

参考文章(15)
J. A. McGeough, Advanced methods of machining ,(1988)
K.H.Zum Gahr, Modelling of two-body abrasive wear Wear. ,vol. 124, pp. 87- 103 ,(1988) , 10.1016/0043-1648(88)90236-0
S.B. Luyckx, W. Barlow-Jones, A. Koursaris, N. Mastrantonis, Healing of cracks in WC-Co in the temperature range 600–800°C International Journal of Refractory Metals & Hard Materials. ,vol. 12, pp. 89- 93 ,(1993) , 10.1016/0263-4368(93)90019-C
C. Rubenstein, The mechanics of grinding International Journal of Machine Tool Design and Research. ,vol. 12, pp. 127- 139 ,(1972) , 10.1016/0020-7357(72)90028-5
M.A. Moore, F.S. King, Abrasive wear of brittle solids Wear. ,vol. 60, pp. 123- 140 ,(1980) , 10.1016/0043-1648(80)90253-7
O. Zelwer, S. Malkin, Grinding of WC-Co Cemented Carbides Journal of Engineering for Industry. ,vol. 102, pp. 209- 220 ,(1980) , 10.1115/1.3183856