摘要: It is shown that the growth behavior of potassium chloride crystals from aqueous solution consistent with Frank mechanism. The altered by presence a few parts per million lead chloride. imputed rate at unit steps inhibited and two‐dimensional nucleation markedly increased effects are complete line adsorption complex containing ion steps.

参考文章(12)
John B Newkirk, Growth of cadmium iodide crystals Acta Metallurgica. ,vol. 3, pp. 121- 125 ,(1955) , 10.1016/0001-6160(55)90078-X
G.W Sears, A growth mechanism for mercury whiskers Acta Metallurgica. ,vol. 3, pp. 361- 366 ,(1955) , 10.1016/0001-6160(55)90041-9
Gerald W. Sears, Effect of Poisons on Crystal Growth The Journal of Chemical Physics. ,vol. 29, pp. 1045- 1048 ,(1958) , 10.1063/1.1744653
G.W Sears, A mechanism of whisker growth Acta Metallurgica. ,vol. 3, pp. 367- 369 ,(1955) , 10.1016/0001-6160(55)90042-0
G. W. Sears, R. V. Coleman, Growth Mechanism of Near‐Perfect Crystals The Journal of Chemical Physics. ,vol. 25, pp. 635- 637 ,(1956) , 10.1063/1.1743017
Gerald W. Sears, Growth of Mercury Platelets from the Vapor The Journal of Chemical Physics. ,vol. 25, pp. 637- 642 ,(1956) , 10.1063/1.1743018
J.B. Newkirk, G.W. Sears, Growth of potassium halide crystals from aqueous solution Acta Metallurgica. ,vol. 3, pp. 110- 111 ,(1955) , 10.1016/0001-6160(55)90031-6
J. J. Gilman, W. G. Johnston, G. W. Sears, Dislocation Etch Pit Formation in Lithium Fluoride Journal of Applied Physics. ,vol. 29, pp. 747- 754 ,(1958) , 10.1063/1.1723277