作者: D. Lisjak , M. Drofenik
DOI: 10.1063/1.1540159
关键词:
摘要: Polycrystalline Zn2U (Ba4Zn2Fe36O60) was synthesized. The high-energy milling of the starting powders activated synthesis at 1100 °C. Energy dispersive spectroscopy supported by x-ray diffraction analysis confirmed that pure synthesized in temperature range 1200–1300 °C. magnetic properties were measured. coercivity varied with conditions, while saturation magnetization independent conditions. Nevertheless, both and different from those basic components crystal structure: M (BaFe12O19) Zn2Y (Ba2Zn2Fe12O22).