Consolidation of cryomilled Al–Si using spark plasma sintering

作者: J. Milligan , R. Gauvin , M. Brochu

DOI: 10.1080/14786435.2013.777816

关键词:

摘要: Cryomilled eutectic aluminum–12% silicon powder was sintered using spark plasma sintering (SPS) to create bulk compacts. The cryomilling serves break up and disperse the phase in a well-distributed Si throughout matrix modify morphology of from plate-like spherical, whilst refining aluminium grain size nanometric level. effects different times temperatures SPS on densification powder, evolution, growth change were investigated. compacts analysed X-ray diffraction, scanning electron microscopy optical microscopy. initial stages appear be highly dependent yield strength powder. An estimate temperature gradient seen bed made calculated near 200 °C at highest point. Al investigated it was...

参考文章(49)
J.R. Davis, Aluminum and Aluminum Alloys ,(1993)
Wang Yucheng, Fu Zhengyi, Study of temperature field in spark plasma sintering Materials Science and Engineering B-advanced Functional Solid-state Materials. ,vol. 90, pp. 34- 37 ,(2002) , 10.1016/S0921-5107(01)00780-2
A.S. Helle, K.E. Easterling, M.F. Ashby, Hot isostatic pressing diagrams : new developments Acta Metallurgica. ,vol. 33, pp. 2163- 2174 ,(1985) , 10.1016/0001-6160(85)90177-4
C. Y. Ho, M. W. Ackerman, K. Y. Wu, T. N. Havill, R. H. Bogaard, R. A. Matula, S. G. Oh, H. M. James, Electrical Resistivity of Ten Selected Binary Alloy Systems Journal of Physical and Chemical Reference Data. ,vol. 12, pp. 183- 322 ,(1983) , 10.1063/1.555684
A.J. Clegg, A.A. Das, Wear of a hypereutectic aluminium-silicon alloy Wear. ,vol. 43, pp. 367- 373 ,(1977) , 10.1016/0043-1648(77)90132-6
Chun-Huei Tsau, Jien-Wei Yeh, The coarsening of silicon particles in a submicron-grained layer-deposited Al-12wt% Si alloy Materials Chemistry and Physics. ,vol. 38, pp. 258- 266 ,(1994) , 10.1016/0254-0584(94)90200-3