摘要: Stannous oxide particles having a methane sulfonic acid dissolution rate of 3.56 g stannous in 8.1 70% 30 seconds at temperature 20 to 25° C. are disclosed, including methods making them. Also disclosed packaged that reduce the formation stannic on surface over time.

参考文章(19)
Matthew L. Grandbois, Process for treating crusty SnO ,(2012)
Matthew L. Grandbois, Process for making SNO ,(2012)
Christian Werner, Jessica Maurer, Christoph Steinberg, Harry Zumaque, Method for the preparation of high purity stannous oxide ,(2012)
Patrice Charvin, Stéphane Abanades, Florent Lemont, Gilles Flamant, Experimental study of SnO2/SnO/Sn thermochemical systems for solar production of hydrogen Aiche Journal. ,vol. 54, pp. 2759- 2767 ,(2008) , 10.1002/AIC.11584
Jean E. Drawdy, Gar B. Hoflund, Steven D. Gardner, Eva Yngvadottir, David R. Schryer, Effect of pretreatment on a platinized tin oxide catalyst used for low-temperature Co oxidation Surface and Interface Analysis. ,vol. 16, pp. 369- 374 ,(1990) , 10.1002/SIA.740160178
記庸 齋藤, Noriyasu Saito, 秀夫 荒井, Hideo Arai, Highly pure tin oxide and its production ,(1998)
Hiroyasu Teranishi, Nobuo Takahashi, Manufacture of stannous oxide ,(1984)
Nobuhiko Edo, Fumio Tanno, Production of stannous oxide having high purity ,(1987)
Katsumi Ogi, Kazuhiro Sakai, Hiroyuki Hasegawa, Kazuyoshi Honda, Yutaka Hayashibe, Preparation of stannous oxide ,(1990)