摘要: By using Au58.74Ni36.50V4.76 at.% filler alloy, a reliable Si3N4/Si3N4 joint was brazed at 1,423 K for 60 min in vacuum. The microstructure of the investigated and analyzed by scanning electron microscope with energy dispersive spectroscopy, transmission microscopy, X-ray diffraction. results indicate that consists three main phases: continuous VN reaction layer between alloy Si3N4 ceramic; an Au[Ni] solid solution as matrix joint; Ni[Si,V] particles distributed homogeneously solution. mechanism formation interfacial structure is discussed.