作者: D.N. Braski , H. Schroeder , H. Ullmaier
DOI: 10.1016/0022-3115(79)90611-1
关键词:
摘要: Foils of the ternary alloy, Fe-17 wt% Cr-17 wt% Ni, were cyclotron-injected with~ 160 at ppm helium and annealed at 1023 K for times up to 1.74 Ms (482 h). Some foils were subjected to tensile stresses which ranged from 9.8 to 27.5 MPa during annealing while others were unstressed. Helium bubbles grew in unstressed specimens at different rates depending on their location in the microstructure; the largest bubbles were found at triple grain junctions, smaller ones on the grain boundaries, and the smallest in the grain matrices. Bubble size in …