Customization of milled zirconia copings for all-ceramic crowns: a clinical report.

作者: Baldwin W. Marchack , Yukiko Futatsuki , Christopher B. Marchack , Shane N. White

DOI: 10.1016/S0022-3913(08)00028-0

关键词:

摘要: Generically milled zirconia copings for all-ceramic crowns may not provide optimal thickness and form the coping or porcelain veneer. This article describes customization of to even controlled with aim decreasing cohesive fracture other failures. A full-contour waxing cut back in conjunction a dual-scan technique was used ensure adequate thickness, adequate, butt joints at porcelain-to-coping junctions. (J Prosthet Dent 2008;99:169-173)

参考文章(26)
Jörg R Strub, Avi Wassermann, Michael Kaiser, Clinical long-term results of VITA In-Ceram Classic crowns and fixed partial dentures: A systematic literature review. International Journal of Prosthodontics. ,vol. 19, pp. 355- 363 ,(2006)
J.Y. Thompson, K.J. Anusavice, A. Naman, H.E. Morris, Fracture Surface Characterization of Clinically Failed All-ceramic Crowns Journal of Dental Research. ,vol. 73, pp. 1824- 1832 ,(1994) , 10.1177/00220345940730120601
J.Robert Kelly, Clinically relevant approach to failure testing of all-ceramic restorations. Journal of Prosthetic Dentistry. ,vol. 81, pp. 652- 661 ,(1999) , 10.1016/S0022-3913(99)70103-4
J. Robert Kelly, Stephen D. Campbell, H. Kent Bowen, Fracture-surface analysis of dental ceramics Journal of Prosthetic Dentistry. ,vol. 62, pp. 536- 541 ,(1989) , 10.1016/0022-3913(89)90075-9
Itzhak Shoher, Aharon E. Whiteman, Reinforced porcelain system: A new concept in ceramometal restorations Journal of Prosthetic Dentistry. ,vol. 50, pp. 489- 496 ,(1983) , 10.1016/0022-3913(83)90567-X
Shane N. White, Angelo A. Caputo, Frank M.A. Vidjak, Robert R. Seghi, Moduli of rupture of layered dental ceramics. Dental Materials. ,vol. 10, pp. 52- 58 ,(1994) , 10.1016/0109-5641(94)90022-1
C.H. Hsueh, G.A. Thompson, O.M. Jadaan, A.A. Wereszczak, P.F. Becher, Analyses of layer-thickness effects in bilayered dental ceramics subjected to thermal stresses and ring-on-ring tests. Dental Materials. ,vol. 24, pp. 9- 17 ,(2008) , 10.1016/J.DENTAL.2006.12.009
John W. McLean, Evolution of dental ceramics in the twentieth century Journal of Prosthetic Dentistry. ,vol. 85, pp. 61- 66 ,(2001) , 10.1067/MPR.2001.112545