作者: Kousuke Yamamoto , Yoshihiro Abe
DOI: 10.1111/J.1151-2916.1998.TB02609.X
关键词:
摘要: A novel porous glass-ceramic with a skeleton of NASICON-type copper(II) titanium phosphate was prepared via the controlled crystallization glass and subsequent chemical leaching resulting dense glass-ceramic. volume-crystallized comprised CuTi2(PO4)3 Cu3(PO4)2, whose surface covered by thin layer CuO, reheating nominal composition 50CuO20TiO230P2O5 (in mol%) in air. When leached dilute HCl, Cu3(PO4)2 CuO phases were dissolved out selectively, cuprous NASICON crystal converted to its cupric type, CuTi4(PO4)6, which left as materials. The specific area average pore radius obtained ∼70 m2/g ∼7 nm, respectively. showed high catalytic activities for dehydration 2-propanol.