Mechanical properties and microstructure of an Al2O3–SiC–TiC composite

作者: B.I Smirnov , V.I Nikolaev , T.S Orlova , V.V Shpeizman , A.R de Arellano-López

DOI: 10.1016/S0921-5093(97)00744-2

关键词: Hot pressingMulliteMaterials scienceFracture toughnessComposite numberFlexural strengthWhiskersComposite materialIndentation hardnessMicrostructure

摘要: The mechanical properties and microstructure of a hard, electrodischarge-machinable composite, Al{sub 2}O{sub 3}-SiC-TiC, were studied. material was fabricated by hot pressing 46.1 vol.% 3} powder, 30.9 SiC whiskers 23.0 TiC powder. Significant reaction occurred between the during processing. resultant composite consisted nearly unreacted particles, 3}, plus smaller concentrations SiC, mullite possibly mixture Al-Si-O-C. exhibited at room temperature an elastic modulus 409.6{+-}0.5 GPa, microhardness values 19-32 indentation fracture toughness (KIC) 9.6{+-}0.6 MPa(m)0.5, compressive strength as high 2.8 GPa in bending {approx}680-825 MPa.

参考文章(17)
Jules L. Routbort, Ron O. Scattergood, Solid Particle Erosion of Ceramics and Ceramic Composites Key Engineering Materials. ,vol. 71, pp. 23- 50 ,(1992) , 10.4028/WWW.SCIENTIFIC.NET/KEM.71.23
L. Wang, M. R. Wixom, L. T. Thompson, Structural and mechanical properties of TiB2 and TiC prepared by self-propagating high-temperature synthesis/dynamic compaction Journal of Materials Science. ,vol. 29, pp. 534- 543 ,(1994) , 10.1007/BF01162518
Hua-Tay Lin, Paul F. Becher, Creep Behavior of a SiC-Whisker-Reinforced Alumina Journal of the American Ceramic Society. ,vol. 73, pp. 1378- 1381 ,(1990) , 10.1111/J.1151-2916.1990.TB05208.X
Antonio R. Arellano-Lopez, Arturo Dominguez-Rodriguez, Kenneth C. Goretta, Jules L. Routbort, Plastic Deformation Mechanisms in SiC‐Whisker‐Reinforced Alumina Journal of the American Ceramic Society. ,vol. 76, pp. 1425- 1432 ,(1993) , 10.1111/J.1151-2916.1993.TB03921.X
A.G. Evans, D.B. Marshall, Overview no. 85 The mechanical behavior of ceramic matrix composites Acta Metallurgica. ,vol. 37, pp. 2567- 2583 ,(1989) , 10.1016/0001-6160(89)90291-5
A. G. EVANS, E. A. CHARLES, Fracture Toughness Determinations by Indentation Journal of the American Ceramic Society. ,vol. 59, pp. 371- 372 ,(1976) , 10.1111/J.1151-2916.1976.TB10991.X
Edward S. Fisher, Murli H. Manghnani, Ji-Fan Wang, Jules L. Routbort, Elastic Properties of Al2O3 and Si3N4 Matrix Composites with SiC Whisker Reinforcement Journal of the American Ceramic Society. ,vol. 75, pp. 908- 914 ,(1992) , 10.1111/J.1151-2916.1992.TB04159.X
Shigetaka WADA, Naoyoshi WATANABE, Toshihiko TANI, Solid Particle Erosion of Brittle Materials (Part 6) Journal of the Ceramic Society of Japan. ,vol. 96, pp. 111- 118 ,(1988) , 10.2109/JCERSJ.96.111
JITENDRA P. SINGH, KENNETH C. GORETTA, D. S. KUPPERMAN, JULES L. ROUTBORT, JAMES F. RHODES, Fracture toughness and strength of SiC-whisker-reinforced Si sub 3 N sub 4 composites Advanced Ceramic Materials. ,vol. 3, pp. 357- 360 ,(1988) , 10.1111/J.1551-2916.1988.TB00234.X
Ming Jiang, K. C. Goretta, Dileep Singh, J. L. Routbort, Solid‐Particle Erosion of an Al2O3‐SiC‐TiC Composite John Wiley & Sons, Ltd. pp. 239- 246 ,(2008) , 10.1002/9780470294437.CH26