摘要: In this study, zirconium oxide coatings were formed on pure by microarc oxidation technique with the electrolytes containing KOH and different amounts of sodium silicate (0-40 gr/lt) for same coating duration 2 hours. The microstructure, surface roughness, phase content chemical composition characterized using scanning electron microscopy, profilometery X-ray diffractometry. It was found that consist monoclinic ZrO2 (m-ZrO2) tetragonal (t-ZrO2) phases addition increasing concentration in electrolyte increases amount t-ZrO2 phase. well adhered to Zr substrate some cracks porosities all concentrations silicate. thickness roughness increased electrolyte. A glaze like Si rich structure its increase rate evident outermost region coating.