作者: Kanda Hiroyuki , Seta Yasuhiro , Ooashi Tatsuya
DOI:
关键词:
摘要: PROBLEM TO BE SOLVED: To provide an indium oxide multi-layer laminate containing different tin concentrations from one another, whose variation of surface resistance is small with excellent acid and adhesiveness. SOLUTION: The transparent electric conductive comprises at least two layers a metal on substrate board, in which the most outer layer contacting surrounding composed or film amount 20 wt.% more relative to indium, 3-10 formed between concentration each tin-containing constant depth direction layer. COPYRIGHT: (C)2005,JPO&NCIPI