作者: Y.L. Su , W.H. Kao
DOI: 10.1361/105994900770346268
关键词:
摘要: In this study, hard coatings (TiN, TiCN, CrN, and CrCN) Me-DLC (Tix%-C:H Crx%-C:H) were deposited on tungsten carbide (WC) substrate by multiarc physical vapor deposition (MAPVD) unbalanced magnetron (UBM) sputtering, respectively. Counterbodies of the AISI 1045 steel cylinder AA7075T651 aluminum used in cylinder-on-disk, line-contact wear mode under dry condition; a counterbody 52100 ball was ball-on-disk, point-contact mode, both lubricated conditions. All tests conducted with reciprocating machine. After tests, most suitable coating for various counterbodies test environments selected. For coating/1045 cylinder, Ti10%-C:H possesses excellent tribological characteristics. coating/7075T651 display resistance. coating/steel ball, CrCN CrN very little On TiN TiCN coatings, special mechanisms material transfer, adhesion wear, fatigue fracture occurred during initial kerosene lubrication.